作者:ATSUHISA IIDA;EIZO MAEDA;SEIJIRO TANAKA;
作者單位:
刊名:Taikabutsu Overseas
ISSN:0285-0028
出版年:2001-01-05
卷:21
期:3
起頁:187
止頁:0
分類號:TQ175
語種:英文
關鍵詞:
內容簡介The main cause of wear of alumina-spinel castables used in steel ladle sidewalls is peeling-off (structural spalling). This wear is caused by crack formation associated with property changes in the slag- penetrated zone. It was found that both the corrosion resistance and the slag penetration resistance were different, depending on the parity of the alumina, resulting in a difference in the peeling-off characteristics in service. The results of the improvement of alumina-spinel castables, based on lab testing and field trials, are discussed in this paper.
所需耐材幣:0